1.1159 (G46Mn4)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Special Steels | Structural Pressure Vessel and Engineering Steels with C < 0,5% |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| SEW835 | 97.73–98.43 | 0.25–0.5 | 0.9–1.2 | < 0.035 | 0.42–0.5 | < 0.035 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| SEW835 |