1.1339 (GS-C25S)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Special Steels | Structural Pressure Vessel and Engineering Steels with Special Requirements |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | V, % | Al, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 97.47–99.5 | 0.3–0.6 | < 1.1 | < 0.3 | < 0.18 | < 0.02 | 0.02–0.07 | < 0.015 | 0.18–0.22 | < 0.01 | < 0.015 |