1.2249 (45SiCrV6)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy Tool Steels | Cr-V, Cr-V-Si, Cr-V-Mn, Cr-V-Mn-Si |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | V, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| 95.41–96.43 | 1.3–1.6 | 0.5–0.7 | 1.3–1.6 | 0.07–0.12 | < 0.035 | 0.4–0.5 | < 0.035 |