1.2355 (50CrMoV13-15)
Classification
| Country |
Section |
Category |
| Germany |
Alloy Tool Steels |
Cr-Mo, Cr-Mo-V, Mo-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| EN ISO 4957 |
92.15–94.4 |
0.2–0.8 |
0.5–0.9 |
3–3.5 |
0.15–0.35 |
< 0.03 |
0.45–0.55 |
< 0.02 |
1.3–1.7 |
Information on suppliers
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
annealing, soft |
248 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |