1.2718 (55NiCr10)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy Tool Steels | With Ni |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| 94.86–95.95 | 0.15–0.3 | 0.4–0.5 | 0.5–0.7 | 2.5–3 | < 0.035 | 0.5–0.57 | < 0.035 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |