1.4377 (X6NiCrNbCe32-27)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Stainless Steel with Ni ≥ 2.5% without Mo, Nb and Ti |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Nb, % |
N, % |
| EN 10095 |
36.355–42.31 |
< 0.3 |
< 1 |
26–28 |
31–33 |
< 0.025 |
0.05–0.1 |
< 0.02 |
0.04–0.08 |
< 0.01 |
0.6–1 |
< 0.11 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| N |
% |
Nitrogen |