1.4572 (GX5CrNiMoNb23-9)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Stainless and Heat Resisting Steels | Stainless Steels with Special Additions |
Chemical composition
| Standard | Fe, % | Cr, % | Ni, % | C, % | Mo, % |
|---|---|---|---|---|---|
| > 63.95 | < 23 | < 9.5 | < 0.05 | < 3.5 |