1.4662 (X2CrNiMnMoCuN24-4-3-2)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Chemical Resistant and High Temp Ni Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| DIN EN 10088-1:2014 |
62.63–70.2 |
< 0.7 |
2.5–4 |
23–25 |
0.1–0.8 |
3–4.5 |
< 0.035 |
< 0.03 |
< 0.005 |
1–2 |
0.2–0.3 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
| X2CrNiMnMoCuN24-4-3-2 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |