1.4836
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Heat Resistant Steels with Ni > = 2.5% |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
W, % |
| ISO 13583-2:2015 |
25.49–36.12 |
1–2 |
0.5–1.5 |
24–27 |
34–37 |
< 0.03 |
0.38–0.45 |
< 0.03 |
< 0.5 |
4–6 |