1.4838
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Stainless and Heat Resisting Steels | Heat Resistant Steels with Ni > = 2.5% |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| ISO 13583-2:2015 | 29.63–39.52 | 1–2 | 0.5–1.5 | 24–27 | < 0.06 | 34–37 | < 0.03 | 0.38–0.45 | < 0.03 | 0.6–1.8 | < 0.5 |
Note: It is possible to replace Ti with other microalloying elements
Information on suppliers
Standards
| Standard | Description |
|---|---|
| ISO 13583-2:2015 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |