1.4861 (X10NiCr32-20)
Additive material 1.4850, 2.4648
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Stainless and Heat Resisting Steels | Heat Resistant Steels with Ni > = 2.5% |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| 41.305–51 | < 1 | < 1.5 | 19–22 | 30–34 | < 0.045 | < 0.12 | < 0.03 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|---|---|
| 20 | 12 | 7900 | 0.5 | 1.04 | |
| 400 | 16 | ||||
| 800 | 17.5 | ||||
| 1000 | 18.5 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$c\cdot 10^{-3}$$ | $$\frac{J}{kg\cdot K}$$ | The specific heat of the material (range 20°C–T) |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |