1.4902 (X14CrMoVNbN10-1)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Materials with Elevated Temperature Properties |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
| SEW555 |
85.536–87.36 |
< 0.1 |
0.4–0.5 |
10–11 |
0.5–0.7 |
0.15–0.25 |
< 0.012 |
< 0.015 |
0.11–0.16 |
< 0.007 |
0.04–0.06 |
1.4–1.6 |
0.04–0.06 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |