1.4928 (G-X12CrNiMoCoVN12)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Materials with Elevated Temperature Properties |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Cr, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| WL |
77.845–83.43 |
< 0.5 |
0.4–1.3 |
1.3–2 |
10.5–12.5 |
2.5–3.2 |
0.25–0.4 |
< 0.03 |
0.1–0.15 |
< 0.03 |
1.5–2 |
0.02–0.045 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |