1.4930 (GX14CrCoMo13-10)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Stainless and Heat Resisting Steels | Materials with Elevated Temperature Properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Co, % | Cr, % | C, % | Mo, % |
|---|---|---|---|---|---|---|---|
| WL | 73.53–76.4 | 0.4–0.7 | 0.5–0.8 | 9.5–10.5 | 12.5–13.5 | 0.1–0.17 | 0.6–0.8 |