1.4943 (X4NiCrTi25-15)
Classification
| Country |
Section |
Category |
| Germany |
Stainless and Heat Resisting Steels |
Materials with Elevated Temperature Properties |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| WL |
49.54–59.697 |
< 1 |
0.003–0.01 |
< 2 |
13.5–16 |
1.7–2 |
24–27 |
0.1–0.5 |
< 0.35 |
< 0.025 |
< 0.06 |
< 0.015 |
1–1.5 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| K66286 |
ЭП674 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |