1.4970 (X10NiCrMoTiB1515)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Stainless and Heat Resisting Steels | Materials with Elevated Temperature Properties |
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Cr, % | Ti, % | Ni, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|
| 64.079–67.167 | 0.25–0.45 | 0.003–0.006 | 1.6–2 | 14.5–15.5 | 0.35–0.55 | 15–16 | < 0.03 | 0.08–0.12 | < 0.015 | 1.05–1.25 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |