1.5310 (8SiTi4)
Additive material 1.4370, 1.4502, 1.4551
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Structural, Pressure Vessel and Engineering Steels | Mn-Ti, Si-Ti |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| 97.73–98.6 | 0.7–1.1 | 0.7–1 | < 0.035 | < 0.1 | < 0.035 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\alpha\cdot 10^{6}$$, $$K^{-1}$$ | $$\varkappa$$, $$\frac{W}{m\cdot K}$$ | $$\rho$$, $$\frac{kg}{m^3}$$ | $$c\cdot 10^{-3}$$, $$\frac{J}{kg\cdot K}$$ | $$R\cdot 10^{-6}$$, $$\Omega\cdot m$$ |
|---|---|---|---|---|---|
| 20 | 35 | 7800 | 0.45 | 0.3 | |
| 400 | 13.5 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\alpha\cdot 10^{6}$$ | $$K^{-1}$$ | Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ | $$\frac{W}{m\cdot K}$$ | Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |
| $$c\cdot 10^{-3}$$ | $$\frac{J}{kg\cdot K}$$ | The specific heat of the material (range 20°C–T) |
| $$R\cdot 10^{-6}$$ | $$\Omega\cdot m$$ | Electrical resistivity |