Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| EN 10216-2 |
97.589–98.838 |
0.1–0.35 |
0.002–0.006 |
0.6–0.8 |
< 0.2 |
< 0.06 |
< 0.3 |
< 0.06 |
< 0.025 |
0.06–0.1 |
< 0.01 |
0.4–0.5 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\epsilon_T$$, % |
$$KV_{L}$$, $$J$$ |
$$KV_{T}$$, $$J$$ |
Treatment |
|
|
|
|
normalization |
540–690 |
400 |
19 |
17 |
40 |
27 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\epsilon_T$$ |
% |
Elongation at break (transverse) |
| $$KV_{L}$$ |
$$J$$ |
Impact energy (longitudinal) |
| $$KV_{T}$$ |
$$J$$ |
Impact energy (transverse) |