1.5708 (12NiCr3-2)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Cr-Ni with Cr < 1.0% |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
| EN 10263-3 |
97.33–98.71 |
< 0.35 |
0.3–0.6 |
0.4–0.7 |
0.5–0.8 |
< 0.035 |
0.09–0.15 |
< 0.035 |