1.6210 (15MnNi6-3)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Ni-Si, Ni-Mn, Ni-Cu |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
N, % |
| SEW028 |
96.551–98.01 |
0.15–0.35 |
< 0.01 |
1.2–1.65 |
< 0.15 |
< 0.02 |
< 0.06 |
0.5–0.85 |
< 0.02 |
0.02–0.055 |
< 0.015 |
< 0.015 |
0.12–0.18 |
< 0.005 |
< 0.004 |
< 0.05 |
< 0.015 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |