1.6211 (16MnNi6-3)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Ni-Si, Ni-Mn, Ni-Cu |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ti, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Nb, % |
N, % |
| SEW028 |
96.686–98.15 |
0.15–0.5 |
1.2–1.65 |
< 0.02 |
0.5–0.85 |
< 0.02 |
< 0.02 |
< 0.025 |
< 0.19 |
< 0.015 |
< 0.004 |
< 0.02 |
Information on suppliers
Standards