1.6308 (18MnMoNi5-5)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Ni-Mo, Ni-Mo-Mn, Ni-Mo-Cu, Ni-Mo-V, Ni-Mn-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| EN 10222-2 |
96.43–97.9 |
< 0.4 |
1.15–1.55 |
0.5–0.8 |
< 0.03 |
< 0.025 |
< 0.2 |
< 0.015 |
0.45–0.55 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$KV_{L}$$, $$J$$ |
$$KV_{T}$$, $$J$$ |
Treatment |
|
|
|
|
moderate hardening |
550–670 |
400 |
20 |
56 |
40 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$KV_{L}$$ |
$$J$$ |
Impact energy (longitudinal) |
| $$KV_{T}$$ |
$$J$$ |
Impact energy (transverse) |