1.6310 (20MnMoNi5-5)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Ni-Mo, Ni-Mo-Mn, Ni-Mo-Cu, Ni-Mo-V, Ni-Mn-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Co, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
Ta, % |
| SEW028 |
96.111–97.57 |
0.15–0.3 |
< 0.011 |
1.2–1.5 |
< 0.03 |
< 0.2 |
< 0.12 |
0.5–0.8 |
< 0.02 |
0.01–0.04 |
< 0.025 |
< 0.012 |
0.17–0.23 |
< 0.008 |
0.4–0.55 |
< 0.013 |
< 0.03 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
| Ta |
% |
Tantalum |