1.6359 (X2NiCoMo18-8-5)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Ni-Mo, Ni-Mo-Mn, Ni-Mo-Cu, Ni-Mo-V, Ni-Mn-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Ca, % |
Mn, % |
Co, % |
Ti, % |
Ni, % |
Zr, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| WL |
66.227–71.05 |
< 0.1 |
< 0.003 |
< 0.05 |
< 0.1 |
7–8.5 |
0.3–0.6 |
17–19 |
< 0.02 |
0.05–0.15 |
< 0.01 |
< 0.03 |
< 0.01 |
4.6–5.2 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Ca |
% |
Calcium |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |