1.6761 (GS-18NiMoCr37)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Structural, Pressure Vessel and Engineering Steels | Cr-Ni-Mo with Mo <0.4% + 3.5% =< Ni < 5%, or Mo>= 0.4% |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cr, % | Cu, % | Ni, % | V, % | Al, % | As, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 95.707–97.51 | 0.3–0.5 | < 0.011 | 0.7–1.1 | 0.3–0.5 | < 0.12 | 0.6–1.1 | < 0.02 | 0.02–0.05 | < 0.025 | < 0.012 | 0.17–0.23 | < 0.01 | 0.4–0.6 | < 0.015 |