1.6780 (15NiCrMo10-6)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Cr-Ni-Mo with Mo <0.4% + 3.5% =< Ni < 5%, or Mo>= 0.4% |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| WW |
93.12–96.43 |
0.15–0.35 |
0.1–0.4 |
1–1.8 |
< 0.02 |
< 0.25 |
2–3.25 |
< 0.03 |
< 0.01 |
0.12–0.16 |
< 0.01 |
0.2–0.6 |