1.6955 (32NiCrMoV10)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Structural, Pressure Vessel and Engineering Steels | Cr-Ni except Groups 57 to 68 |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|
| 93.07–94.64 | 0.15–0.35 | 0.3–0.6 | 1.8–2.1 | 2.5–3 | 0.07–0.12 | < 0.025 | 0.29–0.36 | < 0.025 | 0.25–0.35 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |