Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| SEW555 |
89.323–96.95 |
< 0.15 |
0.3–6.8 |
1–1.3 |
0.5–0.75 |
0.25–0.35 |
< 0.01 |
< 0.01 |
0.25–0.3 |
< 0.007 |
0.75–1 |