Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
P, % |
C, % |
S, % |
|
96.99–98.12 |
< 0.4 |
0.6–0.9 |
0.9–1.2 |
< 0.025 |
0.38–0.45 |
< 0.035 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\epsilon_{L (L_0 = 5.65\sqrt{S_o})}$$, % |
$$R_{eH}$$, $$MPa$$ |
$$\psi$$, % |
$$KV_{L}$$, $$J$$ |
$$KV_{T}$$, $$J$$ |
Treatment |
|
|
< 16 |
|
moderate hardening |
1000–1200 |
11 |
800 |
30 |
30–35 |
22 |
|
|
|
16–40 |
|
moderate hardening |
900–1100 |
12 |
660 |
35 |
|
|
|
|
|
40–100 |
|
moderate hardening |
800–950 |
14 |
560 |
40 |
|
|
|
|
|
|
|
annealing, solid, carbide spheroidization, cold drawn |
610 |
|
|
60 |
|
|
|
|
|
< 8 |
|
moderate hardening |
1000 |
|
|
|
|
|
|
|
|
8–20 |
|
moderate hardening |
900 |
|
|
|
|
|
|
|
|
20–50 |
|
moderate hardening |
800 |
|
|
|
|
|
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
improved machinability |
255 |
|
|
annealing, soft |
241 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_{L (L_0 = 5.65\sqrt{S_o})}$$ |
% |
Elongation at break (longitudinal) (for L0 = 5.65√So) |
| $$R_{eH}$$ |
$$MPa$$ |
Upper yield point |
| $$\psi$$ |
% |
Reduction in cross section on fracture |
| $$KV_{L}$$ |
$$J$$ |
Impact energy (longitudinal) |
| $$KV_{T}$$ |
$$J$$ |
Impact energy (transverse) |