1.7177 (60Cr3)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Cr-Si, Cr-Mn, Cr-Mn-B, Cr-Si-Mn |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
P, % |
C, % |
S, % |
| EN 10089 |
97–98.15 |
< 0.4 |
0.7–1 |
0.6–0.9 |
< 0.025 |
0.55–0.65 |
< 0.025 |
Information on suppliers
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
improved machinability |
280 |
|
|
annealing, soft |
248 |
|
|
annealing, carbide spheroidization |
230 |