1.7346 (11CrMo4-5)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Structural, Pressure Vessel and Engineering Steels | Cr-Mo with Mo ≥ 0.35% |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Al, % | P, % | C, % | S, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|
| 96.65–97.48 | 0.08–0.22 | 0.9–1.15 | 0.95–1.15 | < 0.03 | < 0.015 | 0.11–0.15 | < 0.015 | 0.48–0.62 |