1.7765 (32CrMoV12-10)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Cr-Mo-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
| WW |
93.915–95.85 |
< 0.35 |
< 0.6 |
2.8–3.2 |
0.25–0.35 |
< 0.025 |
0.3–0.35 |
< 0.01 |
0.8–1.2 |