1.8152 (54SiCrV6)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
Cr-Si-V, Cr-Mn-V, Cr-Si-Mn-V |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
V, % |
P, % |
C, % |
S, % |
| EN 10089 |
95.96–97.19 |
1.2–1.6 |
0.5–0.8 |
0.5–0.8 |
0.1–0.2 |
< 0.025 |
0.51–0.59 |
< 0.025 |
Information on suppliers
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
|
|
improved machinability |
280 |
|
|
annealing, soft |
248 |
|
|
annealing, carbide spheroidization |
230 |