1.8939 (S790QL1)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
High Strength Weldable Steels not Intended for Heat Treatment by User |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| SEW090-2 |
94.01–97.3 |
0.2–0.5 |
1.2–1.7 |
0.4–1 |
< 0.2 |
0.7–1.7 |
< 0.12 |
< 0.025 |
< 0.18 |
< 0.015 |
< 0.05 |
0.2–0.5 |