1.8946 (S355J2WP)
Classification
| Country |
Section |
Category |
| Germany |
Structural, Pressure Vessel and Engineering Steels |
High Strength Weldable Steels not Intended for Heat Treatment by User |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
P, % |
C, % |
S, % |
CEV, % |
|
95.63–99.39 |
< 0.75 |
< 1 |
0.3–1.25 |
0.25–0.55 |
0.06–0.15 |
< 0.12 |
< 0.03 |
< 0.52 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\epsilon_{L (L_0 = 80 mm)}$$, % |
$$\epsilon_{L (L_0 = 5.65\sqrt{S_o})}$$, % |
$$KV_{L}$$, $$J$$ |
Treatment |
|
|
< 3 |
|
|
510–680 |
|
|
|
27 |
|
|
|
3–100 |
|
|
470–630 |
|
|
|
|
|
|
|
< 16 |
|
|
|
355 |
|
|
|
|
|
|
16–40 |
|
|
|
345 |
|
|
|
|
|
|
1.5–2 |
|
|
|
|
16 |
|
|
|
|
|
2–2.5 |
|
|
|
|
17 |
|
|
|
|
|
2.5–3 |
|
|
|
|
18 |
|
|
|
|
|
3–40 |
|
|
|
|
|
22 |
|
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| CEV |
% |
Cerium |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_{L (L_0 = 80 mm)}$$ |
% |
Elongation at break (longitudinal) (for L0 = 80 mm) |
| $$\epsilon_{L (L_0 = 5.65\sqrt{S_o})}$$ |
% |
Elongation at break (longitudinal) (for L0 = 5.65√So) |
| $$KV_{L}$$ |
$$J$$ |
Impact energy (longitudinal) |