1.9613 (SAE1070)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Quality Steels | Steels with Average C ≥ 0,55% or Rm ≥ 700 MPa |
Chemical composition
| Standard | Fe, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|
| 98.26–98.75 | 0.6–0.9 | < 0.03 | 0.65–0.76 | < 0.05 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |