2.0332 (CuZn37Pb0.5)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0300-2.0399 |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
ET, % |
| DIN 17660 |
< 0.2 |
< 0.1 |
62–64 |
34.55–37.9 |
< 0.3 |
< 0.05 |
0.1–0.7 |
< 0.1 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
USA |
| ЛС60-1 |
C33500 |
Standards