2.0367
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0300-2.0399 |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|
| DIN 8513 Part 1 | < 0.2 | 0.1–0.3 | < 0.5 | < 0.3 | 59–62 | 36.565–40.9 | < 0.005 | < 0.03 | < 0.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 8513 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Al | % | Aluminium |
| Pb | % | Lead |