2.0375 (CuZn36Pb3)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0300-2.0399 |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
Примеси, % |
| DIN 17660 |
< 0.3 |
< 0.2 |
60–62 |
33.45–37.5 |
< 0.3 |
< 0.05 |
2.5–3.5 |
< 0.2 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| C35330 |
ЛС63-3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Примеси |
% |
Impurities |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |