2.0402 (C38010, CuZn38Pb1.5, CuZn40Pb2)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | Pure Nickel and Cobalt |
Chemical composition
| Standard | Fe, % | Sn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | ET, % |
|---|---|---|---|---|---|---|---|---|
| DIN 17660 | < 0.4 | < 0.3 | 57–59 | 37.1–41.5 | < 0.4 | < 0.1 | 1.5–2.5 | < 0.2 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine | USA |
|---|---|
| мг04у | C38000 |
Standards
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Sn | % | Tin |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |