2.049 (CuZn31Si1)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0400-2.0499 |
Chemical composition
| Standard | Fe, % | Si, % | Cu, % | Zn, % | Ni, % | Pb, % | ET, % |
|---|---|---|---|---|---|---|---|
| DIN 17660 | < 0.4 | 0.7–1.3 | 66–70 | 26.5–33.3 | < 0.5 | < 0.8 | < 0.5 |
Information on suppliers
Analogues
| USA |
|---|
| C69800 |
Standards
| Standard | Description |
|---|---|
| DIN 17660 | |
| DIN 17671 Part 1 | |
| DIN 17671 Part 2 | |
| DIN 17672 Part 1 | |
| DIN 17672 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Si | % | Silicon |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |