2.05 (SoMs64)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0500-2.0599 |
Chemical composition
| Standard |
Fe, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
ET, % |
| DIN 17660 |
2–3.5 |
3.5–5 |
63–65.5 |
17.3–26.5 |
< 0.5 |
5–7 |
< 1 |
< 0.2 |
Information on suppliers
Analogues
| USA |
CIS, Russia, Ukraine |
| C86300 |
CuZn23Al6Mn4Fe3Pb |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |