2.0525 (CuZn38SnAl)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0500-2.0599 |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Cu, % |
Zn, % |
Ni, % |
Al, % |
Pb, % |
As, % |
ET, % |
| DIN 17660 |
0.1–0.4 |
0.3–0.6 |
59–60.7 |
36.05–40 |
0.2–0.5 |
0.1–0.5 |
0.3–0.7 |
< 0.05 |
< 0.5 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
| CuZn38AlFeNiPbSn |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Sn |
% |
Tin |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| As |
% |
Arsenic |