2.0571
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0500-2.0599 |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|---|---|
| DIN 8566 Part 2 | < 1 | < 0.1 | < 0.5 | 0.5–1 | 56–58 | 36.3–42.5 | 1–2 | < 0.1 | < 0.5 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 8566 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |