2.058 (CuZn40MnPb)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0500-2.0599 |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | ET, % |
|---|---|---|---|---|---|---|---|---|---|---|
| DIN 17660 | < 0.5 | < 0.4 | < 0.5 | 0.4–1.8 | 57–59 | 33.7–41.6 | < 1 | < 0.6 | 1–2 | < 0.5 |
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
|---|
| CuZn40Mn1Pb1 |
Standards
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| ET | % | Total other items |
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |