2.0606 (GB-CuZn34Al2)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0600-2.0699 |
Chemical composition
| Standard | Fe, % | Sn, % | Mn, % | Cu, % | Zn, % | Ni, % | Al, % |
|---|---|---|---|---|---|---|---|
| DIN 17656 | 2.5–3.5 | < 0.05 | 3–5 | 55–65 | 21.25–38 | < 2.7 | 1.5–2.5 |
Note: Cu: Cu + Ni
Information on suppliers
Analogues
| USA |
|---|
| C86800 |
Standards
| Standard | Description |
|---|---|
| DIN 17656 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |