2.0711
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0600-2.0699 |
Chemical composition
| Standard | Si, % | Cu, % | Zn, % | Ni, % | Al, % | Pb, % | S, % | Примеси, % |
|---|---|---|---|---|---|---|---|---|
| DIN 8513 Part 1 | 0.1–0.3 | 46–50 | 38.164–45.9 | 8–11 | < 0.005 | < 0.03 | < 0.001 | < 0.5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| DIN 8513 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Примеси | % | Impurities |
| Si | % | Silicon |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Al | % | Aluminium |
| Pb | % | Lead |
| S | % | Sulfur |