2.0742 (CuNi18Zn27)
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0700-2.0799 |
Chemical composition
| Standard |
Fe, % |
Sn, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Pb, % |
ET, % |
| DIN 17663 |
< 0.3 |
< 0.03 |
< 0.5 |
53.5–56.5 |
23.44–29.5 |
17–19 |
< 0.03 |
< 0.2 |