2.0771 (CuNi7Zn39Mn5Pb3)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy DIN 17007−4 | 2.0700-2.0799 |
Chemical composition
| Standard | Fe, % | Mn, % | Cu, % | Zn, % | Ni, % | Pb, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| DIN 17663 | < 0.3 | 4–6 | 44–48 | 33.3–44 | 6–8 | 2–4 | < 0.4 |
Note: Ni: Ni + Co
Information on suppliers
Analogues
| CIS, Russia, Ukraine |
|---|
| CuNi7Zn39Pb3Mn2 |
Standards
| Standard | Description |
|---|---|
| DIN 17663 | |
| DIN 17672 Part 1 | |
| DIN 17672 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Pb | % | Lead |