2.0838
Classification
| Country |
Section |
Category |
| Germany |
Alloy DIN 17007−4 |
2.0800-2.0899 |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Ti, % |
Cu, % |
Ni, % |
Pb, % |
P, % |
C, % |
S, % |
Примеси, % |
| DIN 1733 Part 1 |
0.4–1.2 |
< 0.5 |
0.8–2 |
< 0.5 |
63.195–69.8 |
29–32 |
< 0.02 |
< 0.02 |
< 0.05 |
< 0.015 |
< 0.5 |